Polymer Property : Film Tensile Strength at Break, MD = 2840 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 19.6 MPa
2840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene
LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..
Film Tensile Strength at Break, MD 19.6 MPa
2840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene
LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
Film Tensile Strength at Break, MD 19.6 MPa
2840 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene
LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..