Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 187 MPa
27100 psi
ASTM D882
DuPont Teijin Films Mylar® LB Polyester Film, 92 Gauge (23 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Variet..
Film Tensile Strength at Break, MD 187 MPa
27100 psi
ASTM D882
DuPont Teijin Films Mylar® LBT Polyester Film, 92 Gauge (23 µm)
Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard th..