Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 65 Gauge
Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 80 Gauge
Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 92 Gauge
Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreat..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® O Polyester Film, 300 Gauge
Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® OX Polyester Film, 400 Gauge
Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 100 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 150 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® S Polyester Film, 200 Gauge
Teijin® Tetoron® S is the designation for a family of clear to hazy polyester films. They are general purpose films having good physical and electrical properties. They also have good chemical and..