Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ISO 527-3
Polimeri Europa Riblene® FM 50 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 50 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FM 50 is characterized by optimum optical properties and rigidity.Films manufactured with Riblene FM 50..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ISO 527-3
Polimeri Europa Riblene® FM 53 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 53 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 53 is characterized by optimum optical properties and rigid..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film
The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
Eastman D4028-F Polyethylene  (discontinued **)
D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
Eastman E6838-014F Polyethylene  (discontinued **)
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
Non-oriented film; ASTM D882
Total PPR 8573 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m..
Film Tensile Strength at Break, MD 21.0 - 56.5 MPa
3050 - 8200 psi
Average value: 38.7 MPa Grade Count:23
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
Reliance Industries LLDPE film - Active alumina + zeolite based film
Information provided by Reliance Industries
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
SABIC HP2022 Series Low Density Polyethylene for Blown Film
Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:..