Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 18.5 MPa | 2680 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TS 7045 LDPE - Film - Plastification The Trithene TS 7045 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |