Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | |
Aldrich Single Layer Graphene on PET PET film base with graphene coating; uniform film and excellent thickness consistency. Its transparency combined with electrical conductivity allows it use in many niche applications. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 301H Polyester Film Melinex® 301H is a coextruded film that is one side heat sealable and is able to accept many industrial coatings.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 505 Polyester Film Melinex® 505 is a high clarity polyester film which is pretreated on both sides to promote adhesion to most industrial coating and inks.Approvals: UL 94 VTM-2 - for 1000 gauge (0.26mm) onlyInformat.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 618 Polyester Film, 1000 Gauge Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide ra.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 623 Polyester Film, 1000 Gauge Melinex® 623 is a super clear polyester film pretreated on both surfaces to give superior solvent adhesion and improved handleability.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge Melinex® ST579 is a clear, heat stabilized polyester film that is primed on one surface for adhesion. Typical applications include flexible electronics, touch screens, displays, circuitry, and othe.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® C Polyester Film, 24 Gauge Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 400 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL Polyester Film, 48 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 92 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 1400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1400 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® S1 Polyester Film, 20 Gauge Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® S1 Polyester Film, 25 Gauge Mylar® S1 films are slightly hazy with surfaces tailored to provide excellent handling and product functionality for a variety of industrial end uses. The outstanding tensile properties and thermal.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® S2 Polyester Film, 750 Gauge Mylar® S2 is a slightly hazy film designed for use in the production of drumheads. It has low haze, excellent impact resistance, and balanced physical properties, resulting in consistent tonal qual.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WC Polyester Film, 48 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 680 Polyester Film, 1000 Gauge Melinex® 680 is a super clear polyester film, pretreated on one side to promote adhesion with improved handleability. It is high clarity, non-yellow base with excellent adhesion on the pretreated s.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge Melinex® ST580 is a clear, heat stabilized polyester film that is primed on one surface for enhanced adhesion to UV curable inks and coatings. Typical applications include flexible electronics, tou.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 400 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MDA Polyester Film, 48 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882 |
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® S2 Polyester Film, 1000 Gauge Mylar® S2 is a slightly hazy film designed for use in the production of drumheads. It has low haze, excellent impact resistance, and balanced physical properties, resulting in consistent tonal qual.. |
|||
Film Tensile Strength at Break, MD | 179 MPa | 26000 psi | ASTM D882A |
DuPont Teijin Films Mylar® WC Polyester Film, 400 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |