Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | >= 96.8 MPa | >= 14000 psi | 300 N/10mm |
Dr. D. Mueller Flexiso® DMD FI 14010 00310 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00310 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Film Tensile Strength at Break, MD | 96.5 MPa | 14000 psi | ASTM D882 |
Dow SARAN WRAP™ 18 Plastic Film SARAN WRAP™ 18 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double would roll.. |
|||
Film Tensile Strength at Break, MD | 96.5 MPa | 14000 psi | ASTM D882 |
Dow Saran® 18L Clear Plastic Barrier Film Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow |