Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 76.0 MPa | 11000 psi | ASTM D882 |
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista.. |
|||
Film Tensile Strength at Break, MD | 76.0 MPa | 11000 psi | ASTM D882 |
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista.. |
|||
Film Tensile Strength at Break, MD | 76.0 MPa | 11000 psi | ASTM D882 |
DuPont™ Clysar® RS900 Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, permeable antifog shrink film engineered for food packaging. It forms tight, leak-resistant heat seals. Printable grades (RST900) offer .. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin
(discontinued **) Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018CA Blown Film Resin
(discontinued **) Exceed 2018CA resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals EXXPOL® Technology. The higher melt index makes this polymer ideally sui.. |
|||
Film Tensile Strength at Break, MD | 75.8 - 141 MPa | 11000 - 20500 psi | ASTM D882 |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Film Tensile Strength at Break, MD | 75.8 - 89.6 MPa | 11000 - 13000 psi | ASTM D882 |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Film Tensile Strength at Break, MD | 75.8 - 117 MPa | 11000 - 17000 psi | ASTM D882 |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |
|||
Film Tensile Strength at Break, MD | 75.8 - 110 MPa | 11000 - 16000 psi | ASTM D882 |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exceed™ 1023CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1023CA is a metallocene ethylene-hexene copolymers. The slightly higher stiffness of Exceed 1023CA makes it easier to process on certain filling machinery, whilst still k.. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
Film Tensile Strength at Break, MD | 75.8 MPa | 11000 psi | ASTM D882 |
Dow Saran® 8 Clear Plastic Barrier Film Saran™ 8 is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double wound rolls.Information provi.. |