Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 73.70 MPa | 10690 psi | ASTM D882 |
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications Product Description: Exact 3131 is an ethylene-based hexen plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3131 is designed for both monolayer and multilayer coex.. |