Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 104 MPa | 15100 psi | ASTM D882 |
Solvay Specialty Polymers Ajedium™ Film Thermoplastic Polyimide (PI, TP) TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra.. |