Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 71.0 MPa
10300 psi
ASTM D882
Dow Saran® 560 Vapor Retarder Film
Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 600 gauge. Roll size: 35.5" x 250 long.Informat..
Film Tensile Strength at Break, MD 71.0 MPa
10300 psi
ASTM D882
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su..
Film Tensile Strength at Break, MD 71.0 MPa
10300 psi
ASTM D882
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom..