Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 103.2 MPa | 14970 psi | ASTM D882 |
NatureWorks® Ingeo™ 4032D Film Grade PLA NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce.. |