Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | ASTM D882 |
DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide.. |
|||
Film Tensile Strength at Break, MD | 103 MPa | 14900 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 52LLC210 Preliminary Data Sheet OPP Film Product Description: A clear gloss, surface-printable polyolefin film with enhanced conformability and squeezability for use in face-stock pressure sensitive applications. The proprietary core const.. |