Polymer Property : Elmendorf Tear Strength MD = 400 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
SABIC HP0322N Low Density Polyethylene for Blown Film
Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr..
Elmendorf Tear Strength MD 400 g
400 g
Westlake Mxsten CV CV77515-F Plastomer  (discontinued **)
Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Elmendorf Tear Strength MD 400 g
400 g
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Elmendorf Tear Strength MD 400 g
400 g
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Elmendorf Tear Strength MD 400 g
400 g
Eastman E6838-964F Polyethylene  (discontinued **)
E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
LG Chemical SEETEC BF410 LDPE
Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG ..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
LG Chemical SEETEC BF415 LDPE
Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm..
Elmendorf Tear Strength MD 400 g
400 g
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade
ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com..
Elmendorf Tear Strength MD 400 g
400 g
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade
ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput..
Elmendorf Tear Strength MD 400 g
400 g
ISO 6283-2
Carmel Olefins IPETHENE® 111 Low Density Polyethylene
IPETHENE® 111 is a low density polyethylene extrusion grade, contains no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 111 is used to pr..
Elmendorf Tear Strength MD 400 g
400 g
ISO 6283-2
Carmel Olefins IPETHENE® 113 Low Density Polyethylene
IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and..
Elmendorf Tear Strength MD 400 g
400 g
ASTM D1922
M. Holland Company LL106 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..
Elmendorf Tear Strength MD 400 g
400 g
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..
Elmendorf Tear Strength MD 400 g
400 g
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..