Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Elmendorf Tear Strength MD | 340 g | 340 g | ASTM D1922 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |