Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 288 g
288 g
ASTM D 1922
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin
FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0..