Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 266 g
266 g
ASTM D1922
Dow DOWLEX™ 2077G Linear Low Density Polyethylene
Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow