Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
M. Holland Company MAGMA® LL1091 LLDPE  (discontinued **)
Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland.
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
M. Holland Company MAGMA® LM115-B LLDPE  (discontinued **)
Features: Good Heat Seal, Good Tear Strength, Good ToughnessUses: BlendingProcessing Method: ExtrusionInformation provided by M. Holland.
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
ExxonMobil LD 146.NH Cast Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
ExxonMobil Escorene® LD-144 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym..
Elmendorf Tear Strength MD 260 - 460 g
260 - 460 g
Average value: 367 g Grade Count:3
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
LG Chemical SEETEC EF320 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
ExxonMobil Exceed™ 1023JA Metallocene Polyethylene Resin
Product Description: Exceed 1023JA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1023JA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Elmendorf Tear Strength MD 260 g
260 g
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of ..
Elmendorf Tear Strength MD 260 g
260 g
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045.11 Polyethylene resin is a premier film resin for general purpose packaging applications, ranging from heavy duty applications to high speed, thin gauge applications. It contains high ..
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Elmendorf Tear Strength MD 260 g
260 g
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..
Elmendorf Tear Strength MD 260 g
260 g
ASTM-D1922
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains antiblock, proc..
Elmendorf Tear Strength MD 260 - 600 g
260 - 600 g
Average value: 514 g Grade Count:12
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Elmendorf Tear Strength MD 260 g
260 g
ASTM D638
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ..
Elmendorf Tear Strength MD 260 g
260 g
ASTM D1922
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..