Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 204 g | 204 g | |
Cyclewood Solutions Xylomer™ XM1-GQD Compostable Film Resin 100% biodegradable and compostable thermoplastic. The compostable resin blend performs well compared to LDPE and is BPI certified compostable under ASTM D-6400. Xylomer™ is modified lignin, an ab.. |