Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 15 g | 15 g | Orientation not specified; ASTM D1922 |
DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide.. |
|||
Elmendorf Tear Strength MD | 15 g | 15 g | ASTM D1922 |
LyondellBasell Alathon® L5845 High Density Polyethylene ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg.. |
|||
Elmendorf Tear Strength MD | 15 g @Thickness 0.0254 mm |
15 g @Thickness 0.00100 in |
ASTM D1922 |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |