Polymer Property : Elmendorf Tear Strength MD = 140 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
LyondellBasell Petrothene® NA362176 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene
ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
LyondellBasell Petrothene® NA362005 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin
Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength MD 140 g
140 g
Dow LDPE 752A Low Density Polyethylene, Film Grade
DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu..
Elmendorf Tear Strength MD 140 g
140 g
gF; ASTM D1922
Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Line..
Elmendorf Tear Strength MD 140 g
140 g
gF; ASTM D1922
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene
Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and ..
Elmendorf Tear Strength MD 140 g
140 g
gF; ASTM D1922
Braskem LL218/21 Cast Film Extrusion Linear Low Density Polyethylene
Liners, LDPE and HDPE blends; General use packages; Technical films for automatic packaging.Additives: Antiblock, DInformation provided by Braskem.
Elmendorf Tear Strength MD 140 g
140 g
ASTM-D1922
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer
LL6802N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid ..
Elmendorf Tear Strength MD 140 - 1210 g
140 - 1210 g
Average value: 353 g Grade Count:18
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..