Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | Modified rectangular test specimen; ASTM D1922 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM D1922 |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM-D1922 |
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | gF; ASTM D1922 |
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM-D1922 |
Braskem LL318 LLDPE Cast Film Extrusion Polyethylene Copolymer LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Elmendorf Tear Strength MD | 120 g | 120 g | ASTM-D1922 |
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene LL318 is a linear low-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It was developed for cast film extrusion. Films obtained with this product show good mechanical.. |
|||
Elmendorf Tear Strength MD | 120 - 701 g | 120 - 701 g | Average value: 437 g Grade Count:12 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |