Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 9.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.70 MPa
1410 psi
ASTM D882
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I..
Film Tensile Strength at Yield, MD 9.70 MPa
1410 psi
ASTM D882
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in..
Film Tensile Strength at Yield, MD 9.70 MPa
1410 psi
ASTM D882
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo..
Film Tensile Strength at Yield, MD 9.70 MPa
1410 psi
ASTM D882
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su..
Copyright © lookpolymers.com All Rights Reserved