Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 39.0 MPa | 5660 psi | ASTM D882 |
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness.. |
|||
Film Tensile Strength at Yield, MD | 39.0 MPa | 5660 psi | ASTM D882 |
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Film Tensile Strength at Yield, MD | 39.0 MPa | 5660 psi | ISO 527-3 |
Total XSene® HD55110 High Density Polyethylene - Blown Film HDPE HD55110 is a bimodal high density polyethylene with a particular molecular design developed with Total Petrochemicals Double Loop Technology™.HDPE HD55110 has been especially designed for appl.. |