Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 2600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 17.9 - 20.0 MPa
2600 - 2900 psi
ASTM D882
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film  (discontinued **)
Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell.
Film Tensile Strength at Yield, MD 17.9 MPa
2600 psi
ASTM D882
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin
Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1..
Film Tensile Strength at Yield, MD 17.9 MPa
2600 psi
Dow DOWLEX™ 2036A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2036A Polyethylene resin is a cast film polymer having improved thermal stability for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a for food ..
Copyright © lookpolymers.com All Rights Reserved