Polymer Property : Film Tensile Strength at Yield, MD = 2320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Polimeri Europa Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex CL 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 508 exhibit a good bal..
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene
Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug..
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op..
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene
Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte..
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50..
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ASTM D882
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ASTM D882
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ASTM D882
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.