Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.51 MPa | 1525 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507A Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Film Tensile Strength at Yield, MD | 10.51 MPa | 1525 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Film Tensile Strength at Yield, MD | 10.51 MPa | 1525 psi | ASTM D882 |
Formosa Plastics Formolene® FORMAX® L91507H Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |