Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.2 MPa | 1480 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Film Tensile Strength at Yield, MD | 10.2 MPa | 1480 psi | ASTM D882 |
ExxonMobil LL 1107x93 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |