Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 1100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
ASTM D882
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze..
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
ASTM D882
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim..
Film Tensile Strength at Yield, MD 7.58 MPa
1100 psi
at 2% offset; ASTM D882
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 7.58 MPa
1100 psi
at 2% offset; ASTM D882
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 7.58 MPa
1100 psi
ASTM D882
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend ..
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
Dow DOWLEX™ 2047A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2047A Polyethylene resin is a cast film polymer for high performance stretch cling applications. It provides outstanding tear strength, impact strength and toughness. It complies with U.S. ..
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging ap..
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2247A Polyethylene resin is a cast film polymer for applications requiring outstanding tear strength, impact strength and toughness. This material complies with U.S. FDA Regulation 21 CFR 1..
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
ASTM D882
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..
Copyright © lookpolymers.com All Rights Reserved