Polymer Property : Film Tensile Strength at Yield, MD = 11.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
ASTM D882
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s..
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
ASTM D882
Iran Petrochemical (PCC) 16503 Linear Low Density Polyethylene
16503 is a LLDPE for general purpose cast stretch film grade. The ease of processing and the low gels make 16503 well suited for production of general purpose monolayer or multilayer cast stretch fi..
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade
DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21..
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
ASTM D882
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow