Polymer Property : Limiting Pressure Velocity = 2.60 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 2.60 MPa-m/sec
74200 psi-ft/min
A. Schulman ComAlloy Lubrilon® 637 Nylon 6/6, Carbon Fiber/Molybdenum Disulfide Filled
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..