Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.543 MPa-m/sec | 15500 psi-ft/min | 10 fpm |
Techmer ES Luriblend® PA6 GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |