Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® CJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® 641 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF10 M/TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and PTFE LubricantFeatures: LubricatedAppearance: Natural Col.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | 10 fpm |
Techmer ES Luriblend® PE 5902 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1045 Bearing/Seal PTFE Rulon® 1045 is a dull gold material that has an excellent ability to elongate in a flip seal application. Coupled with excellent frictional characteristics, it offers the added benefit of energy .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 10000 psi-ft/min | |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | Max velocity is 2.0 m/s (400 fpm) |
Saint-Gobain Rulon® AR Bearing/Seal PTFE Rulon® AR is somewhat more flexible than Rulon® LR, hence suitable for seals and bonded coating of slide surfaces. It has many decades of use in automotive shaft seals and fuel metering pump c.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | v = 10m/min |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Limiting Pressure Velocity | 0.350 MPa-m/sec | 9990 psi-ft/min | v = 100m/min |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |