Polymer Property : Limiting Pressure Velocity = 0.00654 MPa-m/sec Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.00638 - 0.00654 MPa-m/sec
182 - 187 psi-ft/min
30 m/min
Polikim EFALON® B-60 PTFE, 60% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
Limiting Pressure Velocity 0.00409 - 0.00654 MPa-m/sec
117 - 187 psi-ft/min
30 m/min
Polikim EFALON® K-25 PTFE, 25% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...
Limiting Pressure Velocity 0.00409 - 0.00654 MPa-m/sec
117 - 187 psi-ft/min
30 m/min
Polikim EFALON® K-35 PTFE, 35% Carbon Filled
K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings...