Polymer Property : Tensile Strength, Yield = 8.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.80 MPa

@Strain 50.0 %
1280 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 8.80 MPa

@Strain 50.0 %
1280 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 8.80 MPa

@Strain 50.0 %
1280 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 8.80 MPa

@Strain 50.0 %
1280 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 8.80 MPa

@Strain 5.00 %
1280 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 8.80 MPa

@Strain 5.00 %
1280 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..