Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.50 MPa @Strain 100 % |
1230 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® M85A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tensile Strength, Yield | 8.50 MPa @Strain 5.00 % |
1230 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |