Mechanical Properties Metric English Comments
Tensile Strength, Yield 448 MPa

@Temperature 177 °C
65000 psi

@Temperature 350 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Tensile Strength, Yield 448 MPa

@Temperature 23.9 °C
65000 psi

@Temperature 75.0 °F
0° Direction, Dry, Autoclave; ASTM D638
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Tensile Strength, Yield 448 MPa

@Temperature 21.1 °C
65000 psi

@Temperature 70.0 °F
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Tensile Strength, Yield 448 MPa

@Thickness 1.57 mm
65000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Tensile Strength, Yield >= 448 MPa

@Diameter 28.57 - 47.63 mm,
Strain 0.200 %
>= 65000 psi

@Diameter 1.125 - 1.875 in,
Strain 0.200 %
ASTM E-8
H.C. Starck Pure Molybdenum AB, Arc-Cast Bar
Arc-Cast BarDescription of Product: This specification covers carbon-deoxidized molybdenum wrought bar produced from ingots consolidated by the H.C. Stark consumable electrode vacuum-arc-casting pr..
Tensile Strength, Yield >= 448 MPa

@Diameter 28.57 - 47.63 mm,
Strain 0.200 %
>= 65000 psi

@Diameter 1.125 - 1.875 in,
Strain 0.200 %
ASTM E-8
H.C. Starck Pure Molybdenum ABL, Arc-Cast, Low Carbon Bar
Description of Product: This specification covers carbon-deoxidized, low-carbon molybdenum wrought bar produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting p..
Tensile Strength, Yield 448 MPa

@Thickness 12.7 mm,
Temperature 260 °C
65000 psi

@Thickness 0.500 in,
Temperature 500 °F
0.2% offset
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 448 MPa

@Thickness 12.7 mm,
Temperature 538 °C
65000 psi

@Thickness 0.500 in,
Temperature 1000 °F
0.2% offset
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 448 MPa

@Thickness 12.7 mm,
Temperature 20.0 °C
65000 psi

@Thickness 0.500 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 448 - 586 MPa

@Strain 0.200 %,
Thickness <=25.4 mm
65000 - 85000 psi

@Strain 0.200 %,
Thickness <=1.00 in
Turned Bars
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..
Tensile Strength, Yield 448 MPa

@Temperature 24.0 °C
65000 psi

@Temperature 75.2 °F
Dry
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel
Tensile Strength, Yield 448 MPa

@Temperature 200 °C
65000 psi

@Temperature 392 °F
short term exposure
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us..
Tensile Strength, Yield 448 MPa

@Temperature 21.1 °C
65000 psi

@Temperature 70.0 °F
0.002
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..
Tensile Strength, Yield 448 MPa

@Strain 0.200 %
65000 psi

@Strain 0.200 %
Transverse Orientation, True Stress/True Strain
AK Steel 13-4 SR® Ferritic Stainless Steel
AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w..
Tensile Strength, Yield <= 448 MPa

@Strain 0.200 %
<= 65000 psi

@Strain 0.200 %
AMS 5542 annealed, sheet
ATI Allegheny Ludlum Altemp® X-750 Nickel-Based superalloy
Characteristics: precipitation hardenable, high strength up to 1300°F, oxidation resistant up to 1800°F. Applications: aerospace, heat treatment fixtures, forming tools, extrusion dies.Information..