Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 40.0 MPa @Temperature 77.0 °C |
5800 psi @Temperature 171 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
ASTM-D638 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r.. |
|||
Tensile Strength, Yield | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding.. |