Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.90 MPa @Strain 10.0 % |
566 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 50.0 % |
566 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 50.0 % |
566 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 5085A Polyether TPU Resin ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 10.0 % |
566 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 10.0 % |
566 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 5.00 % |
566 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 5.00 % |
566 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 3.90 MPa @Strain 10.0 % |
566 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |