Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.00 MPa @Strain 100 % |
725 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 180A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 5.00 MPa @Temperature 149 °C |
725 psi @Temperature 300 °F |
Flatwise Tension |
Hexcel® Redux® 322 Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |