Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 32.0 MPa @Strain 300 % |
4640 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Yield | 32.0 MPa @Strain 100 % |
4640 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tensile Strength, Yield | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®.. |
|||
Tensile Strength, Yield | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r.. |
|||
Tensile Strength, Yield | 32.0 MPa @Temperature 23.0 °C |
4640 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding.. |