Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.14 MPa @Strain 300 % |
455 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |