Polymer Property : Tensile Strength, Yield = 377 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 5.00 %
377 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..