Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 32.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
90°
Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber
Information provided by HexCel
Tensile Strength, Yield 32.0 MPa

@Strain 300 %
4640 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® S98A Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tensile Strength, Yield 32.0 MPa

@Strain 100 %
4640 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh..
Tensile Strength, Yield 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**)
Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®..
Tensile Strength, Yield 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Tensile Strength, Yield 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
Copyright © lookpolymers.com All Rights Reserved