Polymer Property : Tensile Strength, Yield = 3.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.60 MPa

@Strain 50.0 %
522 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 5080A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 300 %
522 psi

@Strain 300 %
ISO 527
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Tensile Strength, Yield 3.60 MPa

@Strain 5.00 %
522 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 3.60 MPa

@Strain 5.00 %
522 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..