Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.7 MPa @Strain 10.0 % |
1840 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |