Polymer Property : Tensile Strength, Yield = 1710 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 11.8 MPa

@Strain 300 %
1710 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 180A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 11.8 MPa

@Strain 10.0 %
1710 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.8 MPa

@Strain 10.0 %
1710 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.8 MPa

@Strain 10.0 %
1710 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EL550 55 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.8 MPa

@Strain 10.0 %
1710 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 11.8 MPa

@Strain 100 %
1710 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 695A15N Polyester Type Polyurethane Elastomer
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes..
Tensile Strength, Yield 11.8 MPa

@Strain 100 %
1710 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 695A15 Polyester Type Polyurethane Elastomer
This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are ..