Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 114 MPa @Strain 1.00 %, Temperature 600 °C |
16500 psi @Strain 1.00 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 114 MPa @Strain 1.00 %, Temperature 600 °C |
16500 psi @Strain 1.00 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 114 MPa @Strain 1.00 %, Temperature 600 °C |
16500 psi @Strain 1.00 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature 100 °C |
16500 psi @Temperature 212 °F |
Conditioned; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature 100 °C |
16500 psi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | >= 114 MPa @Temperature 250 °C |
>= 16500 psi @Temperature 482 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 114 MPa @Temperature -40.0 °C |
16500 psi @Temperature -40.0 °F |
DAM; ASTM D638 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 114 MPa @Thickness 1.57 mm |
16500 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP639 Paper Base Laminate Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature 100 °C |
16500 psi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature 100 °C |
16500 psi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature -40.0 °C |
16500 psi @Temperature -40.0 °F |
ASTM D638 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |
|||
Tensile Strength, Yield | 114 MPa @Temperature 871 °C |
16500 psi @Temperature 1600 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |