Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.5 MPa @Strain 300 % |
2250 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® M88A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tensile Strength, Yield | 15.5 MPa @Strain 300 % |
2250 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |