Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.00 MPa

@Strain 5.00 %
1310 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EB500 50 Shore D, Blow Molding Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 9.00 MPa

@Strain 5.00 %
1310 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® EB500 Polyether Ester Elastomer (European and Asian Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 9.00 MPa

@Strain 50.0 %
1310 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1055DE Poly(adipate)ester TPU Resin
ISOTHANE 1000 Elite series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and t..
Tensile Strength, Yield 9.00 MPa

@Strain 100 %
1310 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1090AE Poly(adipate)ester TPU Resin
ISOTHANE 1000 Elite series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and t..
Tensile Strength, Yield 9.03 MPa

@Strain 100 %
1310 psi

@Strain 100 %
ISO 527
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Tensile Strength, Yield 9.00 MPa

@Strain 100 %
1310 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
Tensile Strength, Yield 9.03 MPa

@Strain 300 %
1310 psi

@Strain 300 %
ASTM D-412
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..
Copyright © lookpolymers.com All Rights Reserved